16MnCr5 1.7131 Alloy Steel Round Bar
16MnCr5 1.7131 Alloy Steel Round Bar
Model
16MnCr5 1.7131

Item specifics

Delivery Condition
normalised and tempered/softened

Review

Description

16MnCr5 1.7131 Alloy Steel

 

Grade :16MnCr5

Number:1.7131

Classification: Alloy special steel

 

Our supply size :

Diameter : 80 to 600 mm ;

Length : 1000 to 9000 mm ;

 

Our advantage :

1. High Quality, Reasonable Price

2. Over 40 Years Experience

3. ISO NQA Certificated Factory

4. Worldwide shipping

5. Emergency Orders and Fast Delivery

 

Equivalent grades of steel 16MnCr5 (1.7131)

EU

USA

Germany

France

England

Italy

EN

-

DIN,WNr

AFNOR

BS

UNI

16MnCr5

SAE5115

16MnCr5

16MC5

527M17

16MnCr5

 

Chemical composition % of steel 16MnCr5 (1.7131): EN 10084-2008

C

Si

Mn

P

S

Cr

0.14 - 0.19

max   0.4

1 - 1.3

max   0.025

max   0.035

0.8 - 1.1

 

Standard:

EN 10084: 2008 Case hardening steels. Technical delivery conditions

EN 10132-2: 2000 Cold rolled narrow steel strip for heat treatment.Case hardening steels

EN 10263-3: 2001 Steel rod, bars and wire for cold heading and cold extrusion.case hardening steels

EN 10297-1: 2003 Seamless circular steel tubes Non-alloy and alloy steel tubes.

 

Applications

DIN 16MnCr5 1.7131 steel is widely used for a variety of applications in the used to the gearings in rotating machinery. Typical applications such as valve bodies, pumps and fittings, the high load of wheel, bolts, double-headed bolts, gears, internal combustion engine. Electric locomotives, machine tools, tractors, steel rolling equipment, boring machine, railway vehicle, and mining machinery transmission shaft on the steel ball, roller and shaft sleeve, etc.

 

Heat treatment

Annealing

Slowly heated to 790-810 and allow enough times, let the steel to be thoroughly heated, Then cool slowly in the furnace. Different annealing ways will get different hardness.The 16MnCr5 will get Hardness MAX 248 HB Brinell hardness

 

Quenching and temperature

Heated slowly to 788°C, Then put in salt-bath furnace keep 1191 to 1204 ℃。quenching by oil get 60 to 66 HRc hardness. High temperature tempering: 650-700℃,cool in air, get hardness 22 to 30HRC. Low temperature tempering: 150-200 ℃, Cool  in ari, get 61-66HRC hardness.

 

Hot work and cold work

DIN 16MnCr5 steel can hot worked at 205 to 538°C, 16MnCr5 can be cold worked using conventional techniques in the annealed or normalized conditions.

 

Smelting Option

1 EAF: Electric Arc Furnace

2 EAF+LF+VD: Refined-smelting and vacuum degassing

3 EAF+ESR: Electro Slag Remelting

4 EAF+PESR: protective atmosphere Electro Slag Remelting

5 VIM+PESR: Vacuum induction melting

 

Forming Option

1 Hot rolling process

2 Hot Forging: Electro-hydraulic; High-speed-hydraulic; Oil-hydraulic; Precision-forging

 

Heat-treatment Option

1 +A: Annealed (full/soft/spheroidizing)

2 +N: Normalized

3 +NT: Normalized and tempered

4 +QT: Quenched and tempered (water/oil)

 

Surface Option

1 Black Surface

2 Grounded: Bright but rough ; Not precision

3 Machining for plate: Bright and precision; Little turning scar

4 Peeled/Turned: Bright and precision; Little turning scar

5 Polished: Very Bright and precision size; Not turning scar

 

Other Services

1 Cutting: Small pieces

2 CNC Machine: Produce as your drawing

3 Package: Bare/Nylon/Canvas/Wooden

4 Payment:T/T, L/C, O/A(request credit)

5 Transport:FOB/CFR/CIF/DDU/DDP (train/ship/Air)

 

Mill test certificate

EN 10204/3.1 with all relevant data reg. chem. composition, mech. properties and results of testing.


KeyWords