16CrMo44 1.7337 AISI A182 F12 Hot Forged Alloy Steel Bar
- Price
- US $1400
- Model
- 16CrMo44 1.7337
- MOQ
- 1 metric ton
Item specifics
- Steel grade
- 16CrMo44/1.7337
- Applications
- aerospace and oil and gas industries
- Heat treatment
- Normalized,Quenching and Tmenpering
- Surface condition
- Black or bright surface
- Standard
- 16CrMo44/1.7337
Review
Description
16CrMo44/1.7337 is a low-alloy steel containing chromium and molybdenum as strengthening elements.It has good mechanical property similiar like Chinese grade 15CrMo. This materail is generally used in the quenched and tempered condition.
This alloy finds many applications as forgings for the aerospace and oil and gas industries, along with myriad uses in the automotive, agricultural and defense industries, Typical uses are forged gears and shafts, spindles, fixtures, jigs and collars.
Equivalent Grade Chemical Composition | ||||||||
National | Grade | C% | Si% | Mn% | Cr% | Mo% | P% | S% |
DIN | 16CrMo44 | 0.13-0.2 | 0.15-0.35 | 0.5-0.8 | 0.9-1.2 | 0.4-0.5 | ≤0.025 | ≤0.035 |
GB | 15CrMo | 0.12-0.18 | 0.17-0.37 | 0.4-0.7 | 0.8-1.1 | 0.4-0.55 | ≤0.035 | ≤ |
Forging of this steel should be carried out between 2200 and 1650 º F (1200 and 900 º C). The lower the finishing temperature from forging, the finer will be the grain size. This alloy should ideally not be forged below 1650 º F (900 º C) and should be slow cooled after forging.
1.Nominal normalizing temperature:840-890°C
2.Hold the temperature for several hours
3.Cooling in the air
Annealing For 16CrMo44
1.Nominal Annealing temperature:680-720°C
2.Cool slowly in the furance
3.Maximum Brinell hardness of 217
Hardening and Tempering(QT) For 16CrMo44
1.Nominal Hardening temperature:850-870°C
2.Hold at this temperature then quench in oil or water
3.Tempering as soon as possible when the temperature low to ambient
4.Heat uniformly to the suitable temperature of 550-640°C
5.keep the material out of the furnace ,then cool in the air
Mechanical Property( for reference only)
1.Tensile strength: 740MPa
2.Yield point: 635MPa
3.Percentage reduction of area after fracture: 50%
4.Elongation after fracture: 17%
5.Impact test (+20°C): Transverse – 27~32J; Longitud – 60~80J
Delivery Condition
1.Shape:Round/Square / Flat/Shafts/Rollers/Blocks
2.Surface condition:Black surface/Bright surface
3.Heat Treatment:Normalized/Annealed/QT
4.Straightness:Max 3mm/m(Enhanced straightness may be available on request)
5.Length:3000-5800mm suitable for 20″container. above 6000mm,suitable for 40″ container
6.Grain Size: 5-8 acc to ASTM E112-96
7.Ultrasonic Standard: Sep1921/ASTM A388/EN 10228-3
8.Non Metallic Inclusion: 2 max acc to ASTM E45 /K4≤20 acc to DIN 50602
9.Forging Ratio: minimum 4 : 1
10.Marking: Grade/Weight/Length/Size/Heat Number
Quality Certification
A material test report(Inspection Certificate EN 10204 3.1) will be provided, documenting the following:
1.Chemical analysis
2.Mechanical properties
3.Surface hardness
4.Non Metallic Inclusion
5.Heat Treatment Process
6.Grain size
7.Forging ratio
8.NDE test method/criteria
16CrMo44/1.7337 alloy steel manufacturers and suppliers,supplied with round rods,square/flat bars,rollers,shafts,blocks and forging pieces.